Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Architectural Coatings

Architectural Coatings
Architectural Coatings RSS Feed RSS

Franklin Tower Re-Clad in Glass and Metal with Wood Grain Finishes

Franklin Tower Re-Clad in Glass and Metal with Wood Grain Finishes

January 16, 2020
No Comments
As a single-source solution, Linetec provided the anodize, paint and specialty wood grain finishes for the aluminum framing members of Franklin Tower's numerous glazing systems.
Read More
What Drives Color Forecasting?

What Drives Color Forecasting?

Kristin Johansson
January 15, 2020
No Comments
Montaha Hidefi, VP of Color Forecasting at the Color Marketing Group (CMG), Color Landing Studio, discusses CMG, the industries it serves, how it forecasts color trends, and what the color predictions are for the coming years.
Read More
pci0120-Convestro-520583064-900.jpg

High-Performance Waterborne Wood Floor Coatings

An Easy-to-Apply, One-Component Formulation with the Physical Properties of a Two-Component Formulation
Eva Tejada Rosales Berta Vega Sanchez Makoto Nakao Steven Reinstadtler Adam Miller
January 10, 2020
No Comments
A new dispersion provides 1K, low-VOC wood floor coatings with the properties of a 2K floor coating.
Read More
Spectroscopic Analysis of Architectural Coatings for Improved Weathering

Spectroscopic Analysis of Architectural Coatings for Improved Weathering

Matt Andersson Karl Booth
January 6, 2020
No Comments
ATR-FTIR offers an attractive incentive to gain more from UVA testing and has the potential to accelerate product development on exterior products.
Read More
PPG Completes COLORFUL COMMUNITIES Project at Union Rescue Mission Facility in Sylmar, California

PPG Completes COLORFUL COMMUNITIES Project at Union Rescue Mission Facility in Sylmar, California

December 5, 2019
No Comments
PPG announced the completion of a COLORFUL COMMUNITIES project at the Union Rescue Mission's (URM) Hope Gardens Family Center.
Read More
ppG

Coatings Add Distinctive Effects to Calgary Central Library Façade

November 1, 2019
No Comments
Custom color formulated by PPG evokes snowflakes, cracked ice on lake.
Read More
pci1019-Corning-AMpowderOnly35134-Lead-900.jpg

Copper-Containing Glass Ceramic with High Antimicrobial Efficacy

Timothy M. Gross Joydeep Lahiri Avantika Golas Jian Luo Florence Verrier Jackie L. Kurzejewski David E. Baker Jie Wang Paul F. Novak Michael J. Snyder
October 9, 2019
One Comment
This article describes an alkali copper aluminoborophosphosilicate glass ceramic material that acts as a sustainable delivery system for Cu+1 ions with high antimicrobial efficacy.
Read More
pci1019-BYK-187003402-900.jpg

When the Film Thickness Does Not Determine the Leveling

Kerstin Vennhoff
October 8, 2019
No Comments
With RHEOBYK-7610, BYK has succeeded in developing a rheology additive which, in addition to the familiar properties, generates a specific viscosity profile.
Read More
specialty chemicals

Specialty Chemicals Snapshot

Kristin Johansson
September 12, 2019
No Comments
Specialty chemicals are used throughout many industries, including coatings. PCI recently asked Jonathan Craig, Vice President Specialty Chemicals at Ascend Performance Materials, to discuss these performance products and the current state of the market.
Read More
pci0919-Clariant-483702288-900.jpg

Improving Outdoor Durability of Wood Coatings

Dr. Mouhcine Kanouni Jean-Yves Desrats
September 10, 2019
No Comments
These new dispersion additives provide excellent outdoor protection for all water-based polymeric binders used in exterior applications such as coatings, grouts and plasters.
Read More
Previous 1 2 … 33 34 35 36 37 38 39 40 41 … 59 60 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

16 Taken to Hospitals After Incident at Massachusetts Coating Facility

Plaque sign on the outside of the United States Environmental Protection Agency

EPA Draft Finds Worker Risks From trans-1,2-Dichloroethylene

Solstice Logo

Solstice, Element Solutions Terminate $14.5B Deal

Webinar custom content box

Events

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing